Ductile iron handbook
Tipo de material:
- 0874331242
Contenidos:
Theory of solidification and graphite growth in ductile iron;Engineering properties, specifications and physical constants of specific ductile irons;Production of ductile ni-resist;Composition of ductile irons;Melting practices for ductile iron production;Selection of charge materials;Desulfurization;Treatment alloys and materials;Magnesium treatment methods;Postinoculation;Foundry practices;Influence of section size on microstructure and mechanical properties;Heat treatment;Ductile iron casting defects;Ductile iron process control;Welding

Biblioteca actual | Signatura topográfica | Estado | Fecha de vencimiento | Código de barras | |
---|---|---|---|---|---|
Koha Ingenieria | 669.018 DUC - Bloque 22 (Navegar estantería(Abre debajo)) | Disponible | 29883 |
Navegando Koha Ingenieria estanterías Cerrar el navegador de estanterías (Oculta el navegador de estanterías)
No hay imagen de cubierta disponible | No hay imagen de cubierta disponible | No hay imagen de cubierta disponible | ||||||
669.018 CAV - Bloque 22 Fisico-química metalúrgica. | 669.018 DEL Diagramas de equilibrio hierro-carbono | 669.018 DON - Bloque 22 Superalloys : A technical guide / | 669.018 DUC - Bloque 22 Ductile iron handbook | 669.018 DUG Bloque 22 The electrical properties of metals and alloys / | 669.018 ELL - Bloque 22 Constitution of binary alloys : First Supplement. | 669.018 FAR Bloque 22 The alloy tree : A guide to low-alloy steels, stainless steels and nickel-base alloys |
Theory of solidification and graphite growth in ductile iron;Engineering properties, specifications and physical constants of specific ductile irons;Production of ductile ni-resist;Composition of ductile irons;Melting practices for ductile iron production;Selection of charge materials;Desulfurization;Treatment alloys and materials;Magnesium treatment methods;Postinoculation;Foundry practices;Influence of section size on microstructure and mechanical properties;Heat treatment;Ductile iron casting defects;Ductile iron process control;Welding